Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (35) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (26) You Searched For: element_names:"Phosphorus" melting-point-solidus:[1900 TO 1950] CLEAR this search X SAVE this search << Page 1 >> 35 Alloys Found Alloy UNS#DesignationActiveView C12510 * Yes C12510 Profile Suppliers of C12510 C14425 Copper (Copper) Yes C14425 Profile Suppliers of C14425 C14500 * Tellurium-Bearing (PTE) Yes C14500 Profile Suppliers of C14500 C14510 * Tellurium-Bearing Yes C14510 Profile Suppliers of C14510 C14520 * Phosphorus-Deoxidized,Tellurium-Bearing (DPTE) Yes C14520 Profile Suppliers of C14520 C14530 * Yes C14530 Profile Suppliers of C14530 C14750 * High Copper Alloy Yes C14750 Profile Suppliers of C14750 C18835 * Yes C18835 Profile Suppliers of C18835 C19000 * Yes C19000 Profile Suppliers of C19000 C19002 * Yes C19002 Profile Suppliers of C19002 C19005 Yes C19005 Profile Suppliers of C19005 C19022 * High Copper Alloy Yes C19022 Profile Suppliers of C19022 C19100 Yes C19100 Profile Suppliers of C19100 C19140 Yes C19140 Profile Suppliers of C19140 C19160 Yes C19160 Profile Suppliers of C19160 C19215 * Yes C19215 Profile Suppliers of C19215 C19217 Yes C19217 Profile Suppliers of C19217 C19419 * CAC19 (High Copper) Yes C19419 Profile Suppliers of C19419 C19800 * Yes C19800 Profile Suppliers of C19800 C19810 * Hig Copper Alloy Yes C19810 Profile Suppliers of C19810 C40820 * Yes C40820 Profile Suppliers of C40820 C40950 * Yes C40950 Profile Suppliers of C40950 C50150 * Copper Tin Phos Zirconium Yes C50150 Profile Suppliers of C50150 C50500 * Phosphor Bronze, 1.25% E Yes C50500 Profile Suppliers of C50500 C50580 * Yes C50580 Profile Suppliers of C50580 C50590 * Yes C50590 Profile Suppliers of C50590 C50725 * Yes C50725 Profile Suppliers of C50725 C61300 * Yes C61300 Profile Suppliers of C61300 C61400 * Yes C61400 Profile Suppliers of C61400 C64750 * Yes C64750 Profile Suppliers of C64750 C64751 Yes C64751 Profile Suppliers of C64751 C64752 Yes C64752 Profile Suppliers of C64752 C64785 * Yes C64785 Profile Suppliers of C64785 C70260 * Yes C70260 Profile Suppliers of C70260 C70315 STOL 94 Yes C70315 Profile Suppliers of C70315 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>