Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (33) Inactive Alloys (2) U.S. EPA Registered Antimicrobial (27) You Searched For: elongation:[0 TO 3] modulus-of-elasticity-in-tension:[15000 TO 16000] CLEAR this search X SAVE this search << Page 1 >> 35 Alloys Found Alloy UNS#DesignationActiveView C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C26000 * Cartridge Brass, 70% Yes C26000 Profile Suppliers of C26000 C26100 * Brass No C26100 Profile Suppliers of C26100 C26130 * Yes C26130 Profile Suppliers of C26130 C26200 * Yes C26200 Profile Suppliers of C26200 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C41300 * Tin Brass Yes C41300 Profile Suppliers of C41300 C42520 * Yes C42520 Profile Suppliers of C42520 C49260 * GEM Brass Yes C49260 Profile Suppliers of C49260 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C51080 * Yes C51080 Profile Suppliers of C51080 C51100 * Yes C51100 Profile Suppliers of C51100 C51180 * Yes C51180 Profile Suppliers of C51180 C51900 * Yes C51900 Profile Suppliers of C51900 C51980 * Yes C51980 Profile Suppliers of C51980 C52100 * Phospher Bronze, 8% C Yes C52100 Profile Suppliers of C52100 C52180 * Yes C52180 Profile Suppliers of C52180 C52400 * Phospher Bronze 10% D Yes C52400 Profile Suppliers of C52400 C52480 * Yes C52480 Profile Suppliers of C52480 C54400 Phosphor Bronze B-2 Yes C54400 Profile Suppliers of C54400 C61900 * Yes C61900 Profile Suppliers of C61900 C62500 * Yes C62500 Profile Suppliers of C62500 C65500 * High-Silicon Bronze A Yes C65500 Profile Suppliers of C65500 C66430 * Yes C66430 Profile Suppliers of C66430 C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 C66710 Yes C66710 Profile Suppliers of C66710 C66900 * Manganese Brass Yes C66900 Profile Suppliers of C66900 C66907 Yes C66907 Profile Suppliers of C66907 C69750 Yes C69750 Profile Suppliers of C69750 C72600 * Copper Nickel No C72600 Profile Suppliers of C72600 C91000 Yes C91000 Profile Suppliers of C91000 C91100 Yes C91100 Profile Suppliers of C91100 C91300 Yes C91300 Profile Suppliers of C91300 C92800 Yes C92800 Profile Suppliers of C92800 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>