Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
10 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C82000 * |
Copper Beryllium 10C | Yes |
C82000 Profile Suppliers of C82000 |
C82200 * |
Copper Beryllium 3C | Yes |
C82200 Profile Suppliers of C82200 |
C89320 * |
Yes |
C89320 Profile Suppliers of C89320 |
|
C89510 * |
SeBiLOY I (EnviroBrass I) | Yes |
C89510 Profile Suppliers of C89510 |
C89845 * |
Copper-Bismuth-Alloy | Yes |
C89845 Profile Suppliers of C89845 |
C95300 * |
Yes |
C95300 Profile Suppliers of C95300 |
|
C95400 * |
Yes |
C95400 Profile Suppliers of C95400 |
|
C95500 * |
Yes |
C95500 Profile Suppliers of C95500 |
|
C95700 * |
Yes |
C95700 Profile Suppliers of C95700 |
|
C95800 * |
Yes |
C95800 Profile Suppliers of C95800 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |