Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (6) You Searched For: elongation:[12 TO 15] gas-shielded-arc-welding:"Excellent" yield-strength:[90 TO 110] CLEAR this search X SAVE this search << Page 1 >> 6 Alloys Found Alloy UNS#DesignationActiveView C40810 * Yes C40810 Profile Suppliers of C40810 C42220 * Yes C42220 Profile Suppliers of C42220 C61500 * Yes C61500 Profile Suppliers of C61500 C63800 * Yes C63800 Profile Suppliers of C63800 C72600 * Copper Nickel No C72600 Profile Suppliers of C72600 C72800 * Yes C72800 Profile Suppliers of C72800 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>