Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (3) You Searched For: elongation:[12 TO 15] rockwell-30t-scale:[65 TO 70] element_names:"Manganese" modulus-of-elasticity-in-tension:[17000 TO 18000] CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C65100 * Low-Silicon Bronze B Yes C65100 Profile Suppliers of C65100 C70600 * Copper-Nickel, 10% Yes C70600 Profile Suppliers of C70600 C74500 * Nickel Silver, 65-10 Yes C74500 Profile Suppliers of C74500 C78200 Yes C78200 Profile Suppliers of C78200 C78270 Nickel Silver (Nickel Silver) Yes C78270 Profile Suppliers of C78270 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>