Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (7) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (7) You Searched For: elongation:[18 TO 21] gas-shielded-arc-welding:"Excellent" oxyacetylene-welding:"Good" CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C10800 * Yes C10800 Profile Suppliers of C10800 C12200 * Phosphorus-Deoxidized, High Residual P (DHP) Yes C12200 Profile Suppliers of C12200 C12210 * Yes C12210 Profile Suppliers of C12210 C19200 * Yes C19200 Profile Suppliers of C19200 C65100 * Low-Silicon Bronze B Yes C65100 Profile Suppliers of C65100 C65500 * High-Silicon Bronze A Yes C65500 Profile Suppliers of C65500 C72900 * Yes C72900 Profile Suppliers of C72900 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>