Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (7) Inactive Alloys (2) U.S. EPA Registered Antimicrobial (9) You Searched For: elongation:[18 TO 21] tensile-strength:[60 TO 70] tensile-strength:[130 TO 140] CLEAR this search X SAVE this search << Page 1 >> 9 Alloys Found Alloy UNS#DesignationActiveView C26000 * Cartridge Brass, 70% Yes C26000 Profile Suppliers of C26000 C26100 * Brass No C26100 Profile Suppliers of C26100 C26130 * Yes C26130 Profile Suppliers of C26130 C26200 * Yes C26200 Profile Suppliers of C26200 C44250 * Yes C44250 Profile Suppliers of C44250 C52100 * Phospher Bronze, 8% C Yes C52100 Profile Suppliers of C52100 C52180 * Yes C52180 Profile Suppliers of C52180 C64400 * Aluminum Bronze No C64400 Profile Suppliers of C64400 C72900 * Yes C72900 Profile Suppliers of C72900 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>