Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (53) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (30) You Searched For: elongation:[18 TO 21] element_names:"Manganese" CLEAR this search X SAVE this search << Page 1 2 >> 53 Alloys Found Alloy UNS#DesignationActiveView C19419 * CAC19 (High Copper) Yes C19419 Profile Suppliers of C19419 C28330 * Low-Lead Yellow Brass Yes C28330 Profile Suppliers of C28330 C49355 * Copper Zinc Bismuth Alloy Yes C49355 Profile Suppliers of C49355 C62400 * Aluminum Bronze,11% Yes C62400 Profile Suppliers of C62400 C63000 * Aluminum Bronze Yes C63000 Profile Suppliers of C63000 C63200 * Aluminum Bronze Yes C63200 Profile Suppliers of C63200 C65100 * Low-Silicon Bronze B Yes C65100 Profile Suppliers of C65100 C65500 * High-Silicon Bronze A Yes C65500 Profile Suppliers of C65500 C65680 Silicon Bronze Yes C65680 Profile Suppliers of C65680 C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 C67340 Yes C67340 Profile Suppliers of C67340 C67400 Yes C67400 Profile Suppliers of C67400 C67420 Yes C67420 Profile Suppliers of C67420 C67500 Manganese Bronze A Yes C67500 Profile Suppliers of C67500 C67600 Yes C67600 Profile Suppliers of C67600 C69240 Yes C69240 Profile Suppliers of C69240 C69710 Yes C69710 Profile Suppliers of C69710 C70270 * Yes C70270 Profile Suppliers of C70270 C70400 * Copper-Nickel, 5% Yes C70400 Profile Suppliers of C70400 C71000 * Copper-Nickel, 20% Yes C71000 Profile Suppliers of C71000 C71950 Yes C71950 Profile Suppliers of C71950 C72500 * Yes C72500 Profile Suppliers of C72500 C72650 * Yes C72650 Profile Suppliers of C72650 C72900 * Yes C72900 Profile Suppliers of C72900 C75200 * Nickel Silver, 65-18 Yes C75200 Profile Suppliers of C75200 C75400 Nickel Silver, 65-15 Yes C75400 Profile Suppliers of C75400 C85910 * Yellow Brass Yes C85910 Profile Suppliers of C85910 C86100 Manganese Bronze Yes C86100 Profile Suppliers of C86100 C86200 Yes C86200 Profile Suppliers of C86200 C86300 Manganese Bronze Yes C86300 Profile Suppliers of C86300 C86400 Manganese Bronze Yes C86400 Profile Suppliers of C86400 C86500 Manganese Bronze Yes C86500 Profile Suppliers of C86500 C86550 Yes C86550 Profile Suppliers of C86550 C86700 Yes C86700 Profile Suppliers of C86700 C87300 * Silicon Bronze Yes C87300 Profile Suppliers of C87300 C87600 * Copper Silcon Alloy Yes C87600 Profile Suppliers of C87600 C87610 * Cast Copper-Silicon Yes C87610 Profile Suppliers of C87610 C87850 * Copper Silicon Alloy Yes C87850 Profile Suppliers of C87850 C89545 Yes C89545 Profile Suppliers of C89545 C89720 * Copper-Bismuth Alloy (TECO) Yes C89720 Profile Suppliers of C89720 C90400 * Tin Bronze Yes C90400 Profile Suppliers of C90400 C90410 * Tin Bronze Yes C90410 Profile Suppliers of C90410 C94800 Yes C94800 Profile Suppliers of C94800 C95400 * Yes C95400 Profile Suppliers of C95400 C95410 * Yes C95410 Profile Suppliers of C95410 C95700 * Yes C95700 Profile Suppliers of C95700 C95800 * Yes C95800 Profile Suppliers of C95800 C97300 Yes C97300 Profile Suppliers of C97300 C97400 Yes C97400 Profile Suppliers of C97400 C97600 Yes C97600 Profile Suppliers of C97600 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 2 >>