You Searched For:
14 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C82200 * |
Copper Beryllium 3C | Yes |
C82200 Profile Suppliers of C82200 |
C83400 |
Yes |
C83400 Profile Suppliers of C83400 |
|
C83600 |
Ounce Metal | Yes |
C83600 Profile Suppliers of C83600 |
C84200 |
Yes |
C84200 Profile Suppliers of C84200 |
|
C84500 |
Yes |
C84500 Profile Suppliers of C84500 |
|
C86500 |
Manganese Bronze | Yes |
C86500 Profile Suppliers of C86500 |
C89320 * |
Yes |
C89320 Profile Suppliers of C89320 |
|
C89833 * |
Copper Bismuth Alloy | Yes |
C89833 Profile Suppliers of C89833 |
C89844 |
Yes |
C89844 Profile Suppliers of C89844 |
|
C90200 |
Yes |
C90200 Profile Suppliers of C90200 |
|
C90300 |
Tin Bronze | Yes |
C90300 Profile Suppliers of C90300 |
C90400 * |
Tin Bronze | Yes |
C90400 Profile Suppliers of C90400 |
C92200 |
Navy M Bronze | Yes |
C92200 Profile Suppliers of C92200 |
C92600 |
Yes |
C92600 Profile Suppliers of C92600 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |