Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (98) Inactive Alloys (5) U.S. EPA Registered Antimicrobial (93) You Searched For: elongation:[3 TO 6] brazing:"Excellent" CLEAR this search X SAVE this search << Page 1 2 3 >> 103 Alloys Found Alloy UNS#DesignationActiveView C10100 * Oxygen-Free-Electronic (OFE) Yes C10100 Profile Suppliers of C10100 C10200 * Oxygen-Free (OF) Yes C10200 Profile Suppliers of C10200 C10300 * Oxygen-Free Copper (OFXLP) Yes C10300 Profile Suppliers of C10300 C10400 * Oxygen-Free with Ag (OFS) Yes C10400 Profile Suppliers of C10400 C10500 * Oxygen-Free with Ag (OFS) Yes C10500 Profile Suppliers of C10500 C10700 * Oxygen-Free with Ag (OFS) Yes C10700 Profile Suppliers of C10700 C10800 * Yes C10800 Profile Suppliers of C10800 C10850 Oxygen-Free with Mg (MOFC-HR) Yes C10850 Profile Suppliers of C10850 C10910 * Yes C10910 Profile Suppliers of C10910 C12000 * Phosphorus-Deoxidized, Low Residual P (DLP) Yes C12000 Profile Suppliers of C12000 C12100 * Phosphorus-Deoxidized, Low Residual P (DLPS) Yes C12100 Profile Suppliers of C12100 C12200 * Phosphorus-Deoxidized, High Residual P (DHP) Yes C12200 Profile Suppliers of C12200 C12210 * Yes C12210 Profile Suppliers of C12210 C14300 * Cadmium Copper, Deoxidized Yes C14300 Profile Suppliers of C14300 C14310 * Cadmium Copper No C14310 Profile Suppliers of C14310 C14530 * Yes C14530 Profile Suppliers of C14530 C15500 * Yes C15500 Profile Suppliers of C15500 C16200 * Cadmium Copper Yes C16200 Profile Suppliers of C16200 C16210 * High Copper Alloy No C16210 Profile Suppliers of C16210 C16500 * Yes C16500 Profile Suppliers of C16500 C18060 Yes C18060 Profile Suppliers of C18060 C18160 Yes C18160 Profile Suppliers of C18160 C18661 * Yes C18661 Profile Suppliers of C18661 C19000 * Yes C19000 Profile Suppliers of C19000 C19040 * CAC5 (High Copper) Yes C19040 Profile Suppliers of C19040 C19050 * SPKFC-5E (High Copper) Yes C19050 Profile Suppliers of C19050 C19170 * KLF170 (High Copper) Yes C19170 Profile Suppliers of C19170 C19200 * Yes C19200 Profile Suppliers of C19200 C19210 * Yes C19210 Profile Suppliers of C19210 C19217 Yes C19217 Profile Suppliers of C19217 C19220 * Yes C19220 Profile Suppliers of C19220 C19240 * Super KFC Yes C19240 Profile Suppliers of C19240 C19250 * SPKFC-5W (High Copper) Yes C19250 Profile Suppliers of C19250 C19280 * Yes C19280 Profile Suppliers of C19280 C19400 * Yes C19400 Profile Suppliers of C19400 C19419 * CAC19 (High Copper) Yes C19419 Profile Suppliers of C19419 C19500 * Yes C19500 Profile Suppliers of C19500 C21000 * Gilding, 95% Yes C21000 Profile Suppliers of C21000 C22000 * Commercial Bronze, 90% Yes C22000 Profile Suppliers of C22000 C22600 * Jewelry Bronze, 87-1/2% Yes C22600 Profile Suppliers of C22600 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C26000 * Cartridge Brass, 70% Yes C26000 Profile Suppliers of C26000 C26100 * Brass No C26100 Profile Suppliers of C26100 C26130 * Yes C26130 Profile Suppliers of C26130 C26200 * Yes C26200 Profile Suppliers of C26200 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C40500 * Penny Bronze Yes C40500 Profile Suppliers of C40500 C40800 * Silicon Brass No C40800 Profile Suppliers of C40800 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 2 3 >>