Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (6) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (4) You Searched For: elongation:[3 TO 6] capacity-for-being-cold-worked:"Poor" CLEAR this search X SAVE this search << Page 1 >> 6 Alloys Found Alloy UNS#DesignationActiveView C15900 * Dispersion Strengthened Coper (C3/11) Yes C15900 Profile Suppliers of C15900 C35600 Extra High Leaded Brass Yes C35600 Profile Suppliers of C35600 C49300 * Lead-Free Bismuth Alloy (Lead-Free) Yes C49300 Profile Suppliers of C49300 C69300 * ECO Brass Yes C69300 Profile Suppliers of C69300 C87870 * Yes C87870 Profile Suppliers of C87870 C87950 Yes C87950 Profile Suppliers of C87950 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>