Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (5) You Searched For: elongation:[3 TO 6] density:[* TO 0.28] CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C61500 * Yes C61500 Profile Suppliers of C61500 C61900 * Yes C61900 Profile Suppliers of C61900 C95400 * Yes C95400 Profile Suppliers of C95400 C95410 * Yes C95410 Profile Suppliers of C95410 C95500 * Yes C95500 Profile Suppliers of C95500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>