Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (27) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (20) You Searched For: elongation:[3 TO 6] electrical-conductivity:[10.0 TO 15.0] CLEAR this search X SAVE this search << Page 1 >> 28 Alloys Found Alloy UNS#DesignationActiveView C46270 Yes C46270 Profile Suppliers of C46270 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C51080 * Yes C51080 Profile Suppliers of C51080 C51900 * Yes C51900 Profile Suppliers of C51900 C51980 * Yes C51980 Profile Suppliers of C51980 C52100 * Phospher Bronze, 8% C Yes C52100 Profile Suppliers of C52100 C52180 * Yes C52180 Profile Suppliers of C52180 C52400 * Phospher Bronze 10% D Yes C52400 Profile Suppliers of C52400 C52480 * Yes C52480 Profile Suppliers of C52480 C61500 * Yes C61500 Profile Suppliers of C61500 C61900 * Yes C61900 Profile Suppliers of C61900 C63800 * Yes C63800 Profile Suppliers of C63800 C70400 * Copper-Nickel, 5% Yes C70400 Profile Suppliers of C70400 C72500 * Yes C72500 Profile Suppliers of C72500 C72600 * Copper Nickel No C72600 Profile Suppliers of C72600 C72670 Yes C72670 Profile Suppliers of C72670 C72700 * Yes C72700 Profile Suppliers of C72700 C72800 * Yes C72800 Profile Suppliers of C72800 C78200 Yes C78200 Profile Suppliers of C78200 C78270 Nickel Silver (Nickel Silver) Yes C78270 Profile Suppliers of C78270 C87950 Yes C87950 Profile Suppliers of C87950 C93700 Bearing Bronze Yes C93700 Profile Suppliers of C93700 C93800 Anti-acid Metal Yes C93800 Profile Suppliers of C93800 C93900 79-6-15 Yes C93900 Profile Suppliers of C93900 C94700 * Cast Nickel-Tin Bronze Yes C94700 Profile Suppliers of C94700 C95400 * Yes C95400 Profile Suppliers of C95400 C95410 * Yes C95410 Profile Suppliers of C95410 C96970 * Yes C96970 Profile Suppliers of C96970 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>