Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (15) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (15) You Searched For: elongation:[3 TO 6] electrical-conductivity:[45.0 TO 50.0] CLEAR this search X SAVE this search << Page 1 >> 15 Alloys Found Alloy UNS#DesignationActiveView C15900 * Dispersion Strengthened Coper (C3/11) Yes C15900 Profile Suppliers of C15900 C17500 * Copper Beryllium Yes C17500 Profile Suppliers of C17500 C17510 * Copper Beryllium Yes C17510 Profile Suppliers of C17510 C19240 * Super KFC Yes C19240 Profile Suppliers of C19240 C19280 * Yes C19280 Profile Suppliers of C19280 C19419 * CAC19 (High Copper) Yes C19419 Profile Suppliers of C19419 C19500 * Yes C19500 Profile Suppliers of C19500 C50500 * Phosphor Bronze, 1.25% E Yes C50500 Profile Suppliers of C50500 C50715 * Yes C50715 Profile Suppliers of C50715 C64725 * Copper Silicon Alloy Yes C64725 Profile Suppliers of C64725 C70230 * Yes C70230 Profile Suppliers of C70230 C70350 * Yes C70350 Profile Suppliers of C70350 C70370 * Yes C70370 Profile Suppliers of C70370 C82000 * Copper Beryllium 10C Yes C82000 Profile Suppliers of C82000 C82200 * Copper Beryllium 3C Yes C82200 Profile Suppliers of C82200 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>