Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (21) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (12) You Searched For: elongation:[3 TO 6] electrical-conductivity:[5.0 TO 10.0] CLEAR this search X SAVE this search << Page 1 >> 21 Alloys Found Alloy UNS#DesignationActiveView C53800 Yes C53800 Profile Suppliers of C53800 C63800 * Yes C63800 Profile Suppliers of C63800 C65400 Yes C65400 Profile Suppliers of C65400 C65500 * High-Silicon Bronze A Yes C65500 Profile Suppliers of C65500 C69300 * ECO Brass Yes C69300 Profile Suppliers of C69300 C69750 Yes C69750 Profile Suppliers of C69750 C70600 * Copper-Nickel, 10% Yes C70600 Profile Suppliers of C70600 C71000 * Copper-Nickel, 20% Yes C71000 Profile Suppliers of C71000 C72200 Yes C72200 Profile Suppliers of C72200 C72900 * Yes C72900 Profile Suppliers of C72900 C73100 * Copper Zinc Nickel Alloy Yes C73100 Profile Suppliers of C73100 C74500 * Nickel Silver, 65-10 Yes C74500 Profile Suppliers of C74500 C75200 * Nickel Silver, 65-18 Yes C75200 Profile Suppliers of C75200 C75400 Nickel Silver, 65-15 Yes C75400 Profile Suppliers of C75400 C75700 * Nickel Silver, 65-12 Yes C75700 Profile Suppliers of C75700 C77000 Nickel Silver, 55-18 Yes C77000 Profile Suppliers of C77000 C78270 Nickel Silver (Nickel Silver) Yes C78270 Profile Suppliers of C78270 C79860 Yes C79860 Profile Suppliers of C79860 C87870 * Yes C87870 Profile Suppliers of C87870 C93700 Bearing Bronze Yes C93700 Profile Suppliers of C93700 C95500 * Yes C95500 Profile Suppliers of C95500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>