Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (156) Inactive Alloys (9) U.S. EPA Registered Antimicrobial (122) You Searched For: elongation:[3 TO 6] element_names:"Iron" CLEAR this search X SAVE this search << Page 1 2 3 4 >> 165 Alloys Found Alloy UNS#DesignationActiveView C10100 * Oxygen-Free-Electronic (OFE) Yes C10100 Profile Suppliers of C10100 C12510 * Yes C12510 Profile Suppliers of C12510 C15715 * Dispersion Strengthened Alloy Yes C15715 Profile Suppliers of C15715 C15720 * Dispersion Strengthned Alloy Yes C15720 Profile Suppliers of C15720 C15900 * Dispersion Strengthened Coper (C3/11) Yes C15900 Profile Suppliers of C15900 C16200 * Cadmium Copper Yes C16200 Profile Suppliers of C16200 C16500 * Yes C16500 Profile Suppliers of C16500 C17400 * Beryllium Copper No C17400 Profile Suppliers of C17400 C17500 * Copper Beryllium Yes C17500 Profile Suppliers of C17500 C17510 * Copper Beryllium Yes C17510 Profile Suppliers of C17510 C18080 Yes C18080 Profile Suppliers of C18080 C18160 Yes C18160 Profile Suppliers of C18160 C18200 Chromium Copper Yes C18200 Profile Suppliers of C18200 C18400 Chromium Copper Yes C18400 Profile Suppliers of C18400 C18610 Yes C18610 Profile Suppliers of C18610 C18661 * Yes C18661 Profile Suppliers of C18661 C19000 * Yes C19000 Profile Suppliers of C19000 C19024 * High Copper Alloy Yes C19024 Profile Suppliers of C19024 C19025 * Yes C19025 Profile Suppliers of C19025 C19027 * NB 115 (High Copper) Yes C19027 Profile Suppliers of C19027 C19040 * CAC5 (High Copper) Yes C19040 Profile Suppliers of C19040 C19050 * SPKFC-5E (High Copper) Yes C19050 Profile Suppliers of C19050 C19100 Yes C19100 Profile Suppliers of C19100 C19140 Yes C19140 Profile Suppliers of C19140 C19160 Yes C19160 Profile Suppliers of C19160 C19170 * KLF170 (High Copper) Yes C19170 Profile Suppliers of C19170 C19200 * Yes C19200 Profile Suppliers of C19200 C19210 * Yes C19210 Profile Suppliers of C19210 C19217 Yes C19217 Profile Suppliers of C19217 C19220 * Yes C19220 Profile Suppliers of C19220 C19240 * Super KFC Yes C19240 Profile Suppliers of C19240 C19250 * SPKFC-5W (High Copper) Yes C19250 Profile Suppliers of C19250 C19280 * Yes C19280 Profile Suppliers of C19280 C19400 * Yes C19400 Profile Suppliers of C19400 C19419 * CAC19 (High Copper) Yes C19419 Profile Suppliers of C19419 C19500 * Yes C19500 Profile Suppliers of C19500 C19710 * Yes C19710 Profile Suppliers of C19710 C19720 * Yes C19720 Profile Suppliers of C19720 C19810 * Hig Copper Alloy Yes C19810 Profile Suppliers of C19810 C21000 * Gilding, 95% Yes C21000 Profile Suppliers of C21000 C22000 * Commercial Bronze, 90% Yes C22000 Profile Suppliers of C22000 C22600 * Jewelry Bronze, 87-1/2% Yes C22600 Profile Suppliers of C22600 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C26000 * Cartridge Brass, 70% Yes C26000 Profile Suppliers of C26000 C26100 * Brass No C26100 Profile Suppliers of C26100 C26130 * Yes C26130 Profile Suppliers of C26130 C26200 * Yes C26200 Profile Suppliers of C26200 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 2 3 4 >>