Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (147) Inactive Alloys (8) U.S. EPA Registered Antimicrobial (109) You Searched For: elongation:[3 TO 6] element_names:"Zinc" CLEAR this search X SAVE this search << Page 1 2 3 4 >> 155 Alloys Found Alloy UNS#DesignationActiveView C10100 * Oxygen-Free-Electronic (OFE) Yes C10100 Profile Suppliers of C10100 C12510 * Yes C12510 Profile Suppliers of C12510 C18020 Yes C18020 Profile Suppliers of C18020 C18045 Yes C18045 Profile Suppliers of C18045 C18145 Yes C18145 Profile Suppliers of C18145 C18400 Chromium Copper Yes C18400 Profile Suppliers of C18400 C19000 * Yes C19000 Profile Suppliers of C19000 C19024 * High Copper Alloy Yes C19024 Profile Suppliers of C19024 C19025 * Yes C19025 Profile Suppliers of C19025 C19027 * NB 115 (High Copper) Yes C19027 Profile Suppliers of C19027 C19040 * CAC5 (High Copper) Yes C19040 Profile Suppliers of C19040 C19050 * SPKFC-5E (High Copper) Yes C19050 Profile Suppliers of C19050 C19100 Yes C19100 Profile Suppliers of C19100 C19140 Yes C19140 Profile Suppliers of C19140 C19160 Yes C19160 Profile Suppliers of C19160 C19170 * KLF170 (High Copper) Yes C19170 Profile Suppliers of C19170 C19200 * Yes C19200 Profile Suppliers of C19200 C19240 * Super KFC Yes C19240 Profile Suppliers of C19240 C19250 * SPKFC-5W (High Copper) Yes C19250 Profile Suppliers of C19250 C19280 * Yes C19280 Profile Suppliers of C19280 C19400 * Yes C19400 Profile Suppliers of C19400 C19419 * CAC19 (High Copper) Yes C19419 Profile Suppliers of C19419 C19500 * Yes C19500 Profile Suppliers of C19500 C19710 * Yes C19710 Profile Suppliers of C19710 C19720 * Yes C19720 Profile Suppliers of C19720 C19810 * Hig Copper Alloy Yes C19810 Profile Suppliers of C19810 C21000 * Gilding, 95% Yes C21000 Profile Suppliers of C21000 C22000 * Commercial Bronze, 90% Yes C22000 Profile Suppliers of C22000 C22600 * Jewelry Bronze, 87-1/2% Yes C22600 Profile Suppliers of C22600 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C26000 * Cartridge Brass, 70% Yes C26000 Profile Suppliers of C26000 C26100 * Brass No C26100 Profile Suppliers of C26100 C26130 * Yes C26130 Profile Suppliers of C26130 C26200 * Yes C26200 Profile Suppliers of C26200 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C32000 Leaded Red Brass Yes C32000 Profile Suppliers of C32000 C34000 Medium Leaded Brass, 64-1/2% Yes C34000 Profile Suppliers of C34000 C34200 High Leaded Brass, 64-1/2% Yes C34200 Profile Suppliers of C34200 C35000 Medium Leaded Brass, 62% Yes C35000 Profile Suppliers of C35000 C35300 High Leaded Brass, 62% Yes C35300 Profile Suppliers of C35300 C35600 Extra High Leaded Brass Yes C35600 Profile Suppliers of C35600 C36000 Free-Cutting Brass Yes C36000 Profile Suppliers of C36000 C36010 Leaded Brass (Free-Cutting Brass) Yes C36010 Profile Suppliers of C36010 C37000 Free-Cutting Muntz Metal Yes C37000 Profile Suppliers of C37000 C37100 Yes C37100 Profile Suppliers of C37100 C40500 * Penny Bronze Yes C40500 Profile Suppliers of C40500 C40800 * Silicon Brass No C40800 Profile Suppliers of C40800 C40810 * Yes C40810 Profile Suppliers of C40810 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 2 3 4 >>