Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (20) Inactive Alloys (2) U.S. EPA Registered Antimicrobial (12) You Searched For: elongation:[3 TO 6] melting-point-liquidus:[1700 TO 1800] CLEAR this search X SAVE this search << Page 1 >> 22 Alloys Found Alloy UNS#DesignationActiveView C17000 * Copper Beryllium Yes C17000 Profile Suppliers of C17000 C17200 * Copper Beryllium Yes C17200 Profile Suppliers of C17200 C17300 Copper Beryllium Yes C17300 Profile Suppliers of C17300 C26000 * Cartridge Brass, 70% Yes C26000 Profile Suppliers of C26000 C26100 * Brass No C26100 Profile Suppliers of C26100 C26130 * Yes C26130 Profile Suppliers of C26130 C26200 * Yes C26200 Profile Suppliers of C26200 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C34000 Medium Leaded Brass, 64-1/2% Yes C34000 Profile Suppliers of C34000 C44250 * Yes C44250 Profile Suppliers of C44250 C44710 Yes C44710 Profile Suppliers of C44710 C44730 Yes C44730 Profile Suppliers of C44730 C53800 Yes C53800 Profile Suppliers of C53800 C68800 * Yes C68800 Profile Suppliers of C68800 C69000 * Copper Zinc No C69000 Profile Suppliers of C69000 C69750 Yes C69750 Profile Suppliers of C69750 C72670 Yes C72670 Profile Suppliers of C72670 C87700 * Silicon Bronze (Silicon Bronze) Yes C87700 Profile Suppliers of C87700 C93700 Bearing Bronze Yes C93700 Profile Suppliers of C93700 C93800 Anti-acid Metal Yes C93800 Profile Suppliers of C93800 C93900 79-6-15 Yes C93900 Profile Suppliers of C93900 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>