Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (16) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (9) You Searched For: elongation:[3 TO 6] melting-point-solidus:[1550 TO 1600] CLEAR this search X SAVE this search << Page 1 >> 16 Alloys Found Alloy UNS#DesignationActiveView C17000 * Copper Beryllium Yes C17000 Profile Suppliers of C17000 C17200 * Copper Beryllium Yes C17200 Profile Suppliers of C17200 C17300 Copper Beryllium Yes C17300 Profile Suppliers of C17300 C46270 Yes C46270 Profile Suppliers of C46270 C52400 * Phospher Bronze 10% D Yes C52400 Profile Suppliers of C52400 C52480 * Yes C52480 Profile Suppliers of C52480 C66900 * Manganese Brass Yes C66900 Profile Suppliers of C66900 C69300 * ECO Brass Yes C69300 Profile Suppliers of C69300 C69750 Yes C69750 Profile Suppliers of C69750 C87870 * Yes C87870 Profile Suppliers of C87870 C87950 Yes C87950 Profile Suppliers of C87950 C89540 Yes C89540 Profile Suppliers of C89540 C89550 * SeBiLOY III (EnviroBrass III) Yes C89550 Profile Suppliers of C89550 C89560 * Copper-Zinc-Bismuth Yes C89560 Profile Suppliers of C89560 C93800 Anti-acid Metal Yes C93800 Profile Suppliers of C93800 C93900 79-6-15 Yes C93900 Profile Suppliers of C93900 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>