Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (63) Inactive Alloys (7) U.S. EPA Registered Antimicrobial (42) You Searched For: elongation:[3 TO 6] oxyacetylene-welding:"Not Recommended" CLEAR this search X SAVE this search << Page 1 2 >> 70 Alloys Found Alloy UNS#DesignationActiveView C11000 * Electrolytic Tough Pitch (ETP) Yes C11000 Profile Suppliers of C11000 C11300 * Tough Pitch with Ag (STP) Yes C11300 Profile Suppliers of C11300 C11400 * Tough Pitch with Ag (STP) Yes C11400 Profile Suppliers of C11400 C11500 * Tough Pitch with Ag (STP) Yes C11500 Profile Suppliers of C11500 C11600 * Tough Pitch with Ag (STP) Yes C11600 Profile Suppliers of C11600 C12500 * Fire-Refined Tough Pitch (FRTP) Yes C12500 Profile Suppliers of C12500 C12510 * Yes C12510 Profile Suppliers of C12510 C12700 * Copper Alloy No C12700 Profile Suppliers of C12700 C12800 * Copper Alloy No C12800 Profile Suppliers of C12800 C12900 * Fire-Refined Tough Pitch with Ag (FRSTP) Yes C12900 Profile Suppliers of C12900 C13000 Copper Alloy No C13000 Profile Suppliers of C13000 C15000 * Zirconium Copper Yes C15000 Profile Suppliers of C15000 C15100 * Yes C15100 Profile Suppliers of C15100 C15500 * Yes C15500 Profile Suppliers of C15500 C15715 * Dispersion Strengthened Alloy Yes C15715 Profile Suppliers of C15715 C15720 * Dispersion Strengthned Alloy Yes C15720 Profile Suppliers of C15720 C15900 * Dispersion Strengthened Coper (C3/11) Yes C15900 Profile Suppliers of C15900 C16500 * Yes C16500 Profile Suppliers of C16500 C17000 * Copper Beryllium Yes C17000 Profile Suppliers of C17000 C17200 * Copper Beryllium Yes C17200 Profile Suppliers of C17200 C17300 Copper Beryllium Yes C17300 Profile Suppliers of C17300 C17400 * Beryllium Copper No C17400 Profile Suppliers of C17400 C17500 * Copper Beryllium Yes C17500 Profile Suppliers of C17500 C17510 * Copper Beryllium Yes C17510 Profile Suppliers of C17510 C18020 Yes C18020 Profile Suppliers of C18020 C18100 Yes C18100 Profile Suppliers of C18100 C18160 Yes C18160 Profile Suppliers of C18160 C18200 Chromium Copper Yes C18200 Profile Suppliers of C18200 C18400 Chromium Copper Yes C18400 Profile Suppliers of C18400 C18500 High Copper No C18500 Profile Suppliers of C18500 C18661 * Yes C18661 Profile Suppliers of C18661 C19040 * CAC5 (High Copper) Yes C19040 Profile Suppliers of C19040 C19050 * SPKFC-5E (High Copper) Yes C19050 Profile Suppliers of C19050 C19140 Yes C19140 Profile Suppliers of C19140 C19160 Yes C19160 Profile Suppliers of C19160 C19170 * KLF170 (High Copper) Yes C19170 Profile Suppliers of C19170 C19240 * Super KFC Yes C19240 Profile Suppliers of C19240 C19250 * SPKFC-5W (High Copper) Yes C19250 Profile Suppliers of C19250 C19419 * CAC19 (High Copper) Yes C19419 Profile Suppliers of C19419 C32000 Leaded Red Brass Yes C32000 Profile Suppliers of C32000 C34000 Medium Leaded Brass, 64-1/2% Yes C34000 Profile Suppliers of C34000 C34200 High Leaded Brass, 64-1/2% Yes C34200 Profile Suppliers of C34200 C35000 Medium Leaded Brass, 62% Yes C35000 Profile Suppliers of C35000 C35300 High Leaded Brass, 62% Yes C35300 Profile Suppliers of C35300 C35600 Extra High Leaded Brass Yes C35600 Profile Suppliers of C35600 C36000 Free-Cutting Brass Yes C36000 Profile Suppliers of C36000 C36010 Leaded Brass (Free-Cutting Brass) Yes C36010 Profile Suppliers of C36010 C37000 Free-Cutting Muntz Metal Yes C37000 Profile Suppliers of C37000 C37100 Yes C37100 Profile Suppliers of C37100 C42200 * Yes C42200 Profile Suppliers of C42200 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 2 >>