Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (14) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (9) You Searched For: elongation:[45 TO 48] capacity-for-being-hot-formed:"Poor" CLEAR this search X SAVE this search << Page 1 >> 14 Alloys Found Alloy UNS#DesignationActiveView C18700 Free-Machining Cu Yes C18700 Profile Suppliers of C18700 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C31400 Leaded Commercial Bronze Yes C31400 Profile Suppliers of C31400 C31600 Leaded Commercial Bronze (Nickel-Bearing) Yes C31600 Profile Suppliers of C31600 C32000 Leaded Red Brass Yes C32000 Profile Suppliers of C32000 C34000 Medium Leaded Brass, 64-1/2% Yes C34000 Profile Suppliers of C34000 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C51100 * Yes C51100 Profile Suppliers of C51100 C51180 * Yes C51180 Profile Suppliers of C51180 C51900 * Yes C51900 Profile Suppliers of C51900 C74500 * Nickel Silver, 65-10 Yes C74500 Profile Suppliers of C74500 C75200 * Nickel Silver, 65-18 Yes C75200 Profile Suppliers of C75200 C75700 * Nickel Silver, 65-12 Yes C75700 Profile Suppliers of C75700 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>