Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
10 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C23000 * |
Red Brass, 85% | Yes |
C23000 Profile Suppliers of C23000 |
C26000 * |
Cartridge Brass, 70% | Yes |
C26000 Profile Suppliers of C26000 |
C26100 * |
Brass | No |
C26100 Profile Suppliers of C26100 |
C26130 * |
Yes |
C26130 Profile Suppliers of C26130 |
|
C33500 |
Low-Leaded Brass | Yes |
C33500 Profile Suppliers of C33500 |
C34000 |
Medium Leaded Brass, 64-1/2% | Yes |
C34000 Profile Suppliers of C34000 |
C35000 |
Medium Leaded Brass, 62% | Yes |
C35000 Profile Suppliers of C35000 |
C35300 |
High Leaded Brass, 62% | Yes |
C35300 Profile Suppliers of C35300 |
C35600 |
Extra High Leaded Brass | Yes |
C35600 Profile Suppliers of C35600 |
C64400 * |
Aluminum Bronze | No |
C64400 Profile Suppliers of C64400 |
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |