Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (49) Inactive Alloys (6) U.S. EPA Registered Antimicrobial (47) You Searched For: elongation:[6 TO 9] rockwell-30t-scale:[60 TO 65] CLEAR this search X SAVE this search << Page 1 2 >> 55 Alloys Found Alloy UNS#DesignationActiveView C64400 * Aluminum Bronze No C64400 Profile Suppliers of C64400 C66430 * Yes C66430 Profile Suppliers of C66430 C66900 * Manganese Brass Yes C66900 Profile Suppliers of C66900 C72500 * Yes C72500 Profile Suppliers of C72500 C75200 * Nickel Silver, 65-18 Yes C75200 Profile Suppliers of C75200 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 2 >>