Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
11 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C10800 * |
Yes |
C10800 Profile Suppliers of C10800 |
|
C12500 * |
Fire-Refined Tough Pitch (FRTP) | Yes |
C12500 Profile Suppliers of C12500 |
C12510 * |
Yes |
C12510 Profile Suppliers of C12510 |
|
C14500 * |
Tellurium-Bearing (PTE) | Yes |
C14500 Profile Suppliers of C14500 |
C14700 * |
Sulfur-Bearing | Yes |
C14700 Profile Suppliers of C14700 |
C14710 * |
Copper Alloy | No |
C14710 Profile Suppliers of C14710 |
C14720 |
Copper Alloy | No |
C14720 Profile Suppliers of C14720 |
C15100 * |
Yes |
C15100 Profile Suppliers of C15100 |
|
C15715 * |
Dispersion Strengthened Alloy | Yes |
C15715 Profile Suppliers of C15715 |
C16200 * |
Cadmium Copper | Yes |
C16200 Profile Suppliers of C16200 |
C16210 * |
High Copper Alloy | No |
C16210 Profile Suppliers of C16210 |
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |