Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (63) Inactive Alloys (16) U.S. EPA Registered Antimicrobial (40) You Searched For: gas-shielded-arc-welding:"Fair" coated-metal-arc-welding:"Not Recommended" CLEAR this search X SAVE this search << Page 1 2 >> 79 Alloys Found Alloy UNS#DesignationActiveView C11000 * Electrolytic Tough Pitch (ETP) Yes C11000 Profile Suppliers of C11000 C11300 * Tough Pitch with Ag (STP) Yes C11300 Profile Suppliers of C11300 C11400 * Tough Pitch with Ag (STP) Yes C11400 Profile Suppliers of C11400 C11500 * Tough Pitch with Ag (STP) Yes C11500 Profile Suppliers of C11500 C11600 * Tough Pitch with Ag (STP) Yes C11600 Profile Suppliers of C11600 C12500 * Fire-Refined Tough Pitch (FRTP) Yes C12500 Profile Suppliers of C12500 C12510 * Yes C12510 Profile Suppliers of C12510 C12700 * Copper Alloy No C12700 Profile Suppliers of C12700 C12800 * Copper Alloy No C12800 Profile Suppliers of C12800 C12900 * Fire-Refined Tough Pitch with Ag (FRSTP) Yes C12900 Profile Suppliers of C12900 C13000 Copper Alloy No C13000 Profile Suppliers of C13000 C14500 * Tellurium-Bearing (PTE) Yes C14500 Profile Suppliers of C14500 C14510 * Tellurium-Bearing Yes C14510 Profile Suppliers of C14510 C14520 * Phosphorus-Deoxidized,Tellurium-Bearing (DPTE) Yes C14520 Profile Suppliers of C14520 C16500 * Yes C16500 Profile Suppliers of C16500 C26100 * Brass No C26100 Profile Suppliers of C26100 C26130 * Yes C26130 Profile Suppliers of C26130 C26200 * Yes C26200 Profile Suppliers of C26200 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C27250 Yes C27250 Profile Suppliers of C27250 C27400 * Yellow Brass, 63% Yes C27400 Profile Suppliers of C27400 C27450 Yellow Brass Yes C27450 Profile Suppliers of C27450 C27451 Yellow Brass (Yellow Brass) Yes C27451 Profile Suppliers of C27451 C27453 Copper Zinc Alloy Yes C27453 Profile Suppliers of C27453 C27460 Yes C27460 Profile Suppliers of C27460 C27550 Yes C27550 Profile Suppliers of C27550 C28000 * Muntz Metal, 60% Yes C28000 Profile Suppliers of C28000 C28340 Yes C28340 Profile Suppliers of C28340 C28500 Copper-Zinc- Alloy (Brass) Yes C28500 Profile Suppliers of C28500 C28550 Yes C28550 Profile Suppliers of C28550 C33000 Low Leaded Brass (Tube) Yes C33000 Profile Suppliers of C33000 C33100 Leaded Brass No C33100 Profile Suppliers of C33100 C33200 High Leaded Brass (Tube) Yes C33200 Profile Suppliers of C33200 C33500 Low-Leaded Brass Yes C33500 Profile Suppliers of C33500 C36300 Copper-Zinc-Lead Alloy Yes C36300 Profile Suppliers of C36300 C36500 Leaded Muntz Metal, Uninhibited Yes C36500 Profile Suppliers of C36500 C36600 Leaded Muntz Metal, Arsinical No C36600 Profile Suppliers of C36600 C36700 Leaded Muntz Metal, Antimonial No C36700 Profile Suppliers of C36700 C36800 Leaded Brass No C36800 Profile Suppliers of C36800 C41300 * Tin Brass Yes C41300 Profile Suppliers of C41300 C43500 * Tin Brass Yes C43500 Profile Suppliers of C43500 C44300 * Admiralty, Arsenical Yes C44300 Profile Suppliers of C44300 C44400 * Admiralty, Antimonial Yes C44400 Profile Suppliers of C44400 C44500 * Admiralty, Phosphorized Yes C44500 Profile Suppliers of C44500 C44730 Yes C44730 Profile Suppliers of C44730 C46400 Naval Brass, Uninhibited Yes C46400 Profile Suppliers of C46400 C46500 Naval Brass, Arsenical Yes C46500 Profile Suppliers of C46500 C46600 Tin Brass No C46600 Profile Suppliers of C46600 C46700 Tin Brass No C46700 Profile Suppliers of C46700 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 2 >>