Alloy UNS# | Designation | Active | View |
---|---|---|---|
C10100 * |
Oxygen-Free-Electronic (OFE) | Yes |
C10100 Profile Suppliers of C10100 |
C10200 * |
Oxygen-Free (OF) | Yes |
C10200 Profile Suppliers of C10200 |
C10400 * |
Oxygen-Free with Ag (OFS) | Yes |
C10400 Profile Suppliers of C10400 |
C10500 * |
Oxygen-Free with Ag (OFS) | Yes |
C10500 Profile Suppliers of C10500 |
C10700 * |
Oxygen-Free with Ag (OFS) | Yes |
C10700 Profile Suppliers of C10700 |
C10910 * |
Yes |
C10910 Profile Suppliers of C10910 |
|
C23000 * |
Red Brass, 85% | Yes |
C23000 Profile Suppliers of C23000 |
C26000 * |
Cartridge Brass, 70% | Yes |
C26000 Profile Suppliers of C26000 |
C41500 * |
Tin Brass | Yes |
C41500 Profile Suppliers of C41500 |
C42500 * |
Yes |
C42500 Profile Suppliers of C42500 |
|