Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (21) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (21) You Searched For: gas-shielded-arc-welding:"Good" rockwell-30t-scale:[60 TO 65] CLEAR this search X SAVE this search << Page 1 >> 22 Alloys Found Alloy UNS#DesignationActiveView C10100 * Oxygen-Free-Electronic (OFE) Yes C10100 Profile Suppliers of C10100 C10200 * Oxygen-Free (OF) Yes C10200 Profile Suppliers of C10200 C10400 * Oxygen-Free with Ag (OFS) Yes C10400 Profile Suppliers of C10400 C10500 * Oxygen-Free with Ag (OFS) Yes C10500 Profile Suppliers of C10500 C10700 * Oxygen-Free with Ag (OFS) Yes C10700 Profile Suppliers of C10700 C10910 * Yes C10910 Profile Suppliers of C10910 C17300 Copper Beryllium Yes C17300 Profile Suppliers of C17300 C21000 * Gilding, 95% Yes C21000 Profile Suppliers of C21000 C22000 * Commercial Bronze, 90% Yes C22000 Profile Suppliers of C22000 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C26000 * Cartridge Brass, 70% Yes C26000 Profile Suppliers of C26000 C40500 * Penny Bronze Yes C40500 Profile Suppliers of C40500 C40800 * Silicon Brass No C40800 Profile Suppliers of C40800 C41100 * Tin Brass Yes C41100 Profile Suppliers of C41100 C41500 * Tin Brass Yes C41500 Profile Suppliers of C41500 C43000 * Tin Brass Yes C43000 Profile Suppliers of C43000 C43400 * Yes C43400 Profile Suppliers of C43400 C50500 * Phosphor Bronze, 1.25% E Yes C50500 Profile Suppliers of C50500 C51100 * Yes C51100 Profile Suppliers of C51100 C66430 * Yes C66430 Profile Suppliers of C66430 C72500 * Yes C72500 Profile Suppliers of C72500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>