Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (16) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (17) You Searched For: gas-shielded-arc-welding:"Good" rockwell-30t-scale:[70 TO 75] CLEAR this search X SAVE this search << Page 1 >> 17 Alloys Found Alloy UNS#DesignationActiveView C17000 * Copper Beryllium Yes C17000 Profile Suppliers of C17000 C17200 * Copper Beryllium Yes C17200 Profile Suppliers of C17200 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C26000 * Cartridge Brass, 70% Yes C26000 Profile Suppliers of C26000 C40500 * Penny Bronze Yes C40500 Profile Suppliers of C40500 C40800 * Silicon Brass No C40800 Profile Suppliers of C40800 C41100 * Tin Brass Yes C41100 Profile Suppliers of C41100 C41500 * Tin Brass Yes C41500 Profile Suppliers of C41500 C42500 * Yes C42500 Profile Suppliers of C42500 C43000 * Tin Brass Yes C43000 Profile Suppliers of C43000 C43400 * Yes C43400 Profile Suppliers of C43400 C50500 * Phosphor Bronze, 1.25% E Yes C50500 Profile Suppliers of C50500 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C51100 * Yes C51100 Profile Suppliers of C51100 C52100 * Phospher Bronze, 8% C Yes C52100 Profile Suppliers of C52100 C66430 * Yes C66430 Profile Suppliers of C66430 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>