Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (0) You Searched For: gas-shielded-arc-welding:"Not Recommended" gassing:"Low" CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C85200 Leaded Yellow Brass Yes C85200 Profile Suppliers of C85200 C85500 Yes C85500 Profile Suppliers of C85500 C85700 Leaded Yellow Brass Yes C85700 Profile Suppliers of C85700 C85800 Yes C85800 Profile Suppliers of C85800 C87900 Copper Silicon Yes C87900 Profile Suppliers of C87900 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>