Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (22) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (16) You Searched For: gassing:"Medium" element_names:"Manganese" CLEAR this search X SAVE this search << Page 1 >> 22 Alloys Found Alloy UNS#DesignationActiveView C84000 * Semi-Red Brass Yes C84000 Profile Suppliers of C84000 C84010 * Semi-Red Brass Yes C84010 Profile Suppliers of C84010 C84020 * Semi-Red Brass Yes C84020 Profile Suppliers of C84020 C84030 * Low Lead Semi-Red Brass Yes C84030 Profile Suppliers of C84030 C85430 Yes C85430 Profile Suppliers of C85430 C86550 Yes C86550 Profile Suppliers of C86550 C87800 * Cast Silicon Bronze Yes C87800 Profile Suppliers of C87800 C89545 Yes C89545 Profile Suppliers of C89545 C90400 * Tin Bronze Yes C90400 Profile Suppliers of C90400 C90410 * Tin Bronze Yes C90410 Profile Suppliers of C90410 C90420 * Tin Bronze Yes C90420 Profile Suppliers of C90420 C94700 * Cast Nickel-Tin Bronze Yes C94700 Profile Suppliers of C94700 C94800 Yes C94800 Profile Suppliers of C94800 C95400 * Yes C95400 Profile Suppliers of C95400 C95500 * Yes C95500 Profile Suppliers of C95500 C95700 * Yes C95700 Profile Suppliers of C95700 C95800 * Yes C95800 Profile Suppliers of C95800 C96300 * Yes C96300 Profile Suppliers of C96300 C97300 Yes C97300 Profile Suppliers of C97300 C97400 Yes C97400 Profile Suppliers of C97400 C99760 * Yes C99760 Profile Suppliers of C99760 C99770 * Yes C99770 Profile Suppliers of C99770 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>