Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (9) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (6) You Searched For: melting-point-liquidus:[1900 TO 2000] tensile-strength:[140 TO 150] CLEAR this search X SAVE this search << Page 1 >> 9 Alloys Found Alloy UNS#DesignationActiveView C17540 CW103C Yes C17540 Profile Suppliers of C17540 C19910 * NKT 322 (High Copper) Yes C19910 Profile Suppliers of C19910 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C61500 * Yes C61500 Profile Suppliers of C61500 C61800 * Yes C61800 Profile Suppliers of C61800 C61900 * Yes C61900 Profile Suppliers of C61900 C64752 Yes C64752 Profile Suppliers of C64752 C70252 * Copper Nickel (NKC 388) Yes C70252 Profile Suppliers of C70252 C77000 Nickel Silver, 55-18 Yes C77000 Profile Suppliers of C77000 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>