Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (8) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (5) You Searched For: melting-point-solidus:[1800 TO 1850] element_names:"Manganese" CLEAR this search X SAVE this search << Page 1 >> 8 Alloys Found Alloy UNS#DesignationActiveView C42230 Yes C42230 Profile Suppliers of C42230 C63800 * Yes C63800 Profile Suppliers of C63800 C64200 * Aluminum Bronze Yes C64200 Profile Suppliers of C64200 C69100 * Yes C69100 Profile Suppliers of C69100 C69150 * Copper Zinc Alloy (Copper Zinc Alloy) Yes C69150 Profile Suppliers of C69150 C73100 * Copper Zinc Nickel Alloy Yes C73100 Profile Suppliers of C73100 C76200 Nickel Silver Yes C76200 Profile Suppliers of C76200 C97300 Yes C97300 Profile Suppliers of C97300 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>