Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (24) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (24) You Searched For: modulus-of-elasticity-in-tension:[14000 TO 15000] antimicrobial:"true" CLEAR this search X SAVE this search << Page 1 >> 24 Alloys Found Alloy UNS#DesignationActiveView C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C27200 * Yellow Brass Yes C27200 Profile Suppliers of C27200 C27400 * Yellow Brass, 63% Yes C27400 Profile Suppliers of C27400 C28000 * Muntz Metal, 60% Yes C28000 Profile Suppliers of C28000 C45470 * Copper-Zinc-Tin Aluminum Alloy Yes C45470 Profile Suppliers of C45470 C49250 * Copper-Zinc-Bismuth (Copper-Zinc-Bismuth) Yes C49250 Profile Suppliers of C49250 C49300 * Lead-Free Bismuth Alloy (Lead-Free) Yes C49300 Profile Suppliers of C49300 C49340 * GEM Brass Yes C49340 Profile Suppliers of C49340 C49350 * Bismuth Brass Alloy Yes C49350 Profile Suppliers of C49350 C65500 * High-Silicon Bronze A Yes C65500 Profile Suppliers of C65500 C66908 * Copper-Zinc-Manganese Yes C66908 Profile Suppliers of C66908 C66910 * Copper-Zinc-Manganese Yes C66910 Profile Suppliers of C66910 C66913 * Copper-Zinc-Manganese Yes C66913 Profile Suppliers of C66913 C66915 * Copper-Zinc-Manganese Yes C66915 Profile Suppliers of C66915 C66925 * Copper-Zinc-Manganese Yes C66925 Profile Suppliers of C66925 C69220 * Copper Zinc Alloy Yes C69220 Profile Suppliers of C69220 C74400 * Nickel Silver Yes C74400 Profile Suppliers of C74400 C84000 * Semi-Red Brass Yes C84000 Profile Suppliers of C84000 C84010 * Semi-Red Brass Yes C84010 Profile Suppliers of C84010 C84030 * Low Lead Semi-Red Brass Yes C84030 Profile Suppliers of C84030 C94700 * Cast Nickel-Tin Bronze Yes C94700 Profile Suppliers of C94700 C95200 * Yes C95200 Profile Suppliers of C95200 C95600 * Yes C95600 Profile Suppliers of C95600 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>