Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (48) Inactive Alloys (5) U.S. EPA Registered Antimicrobial (7) You Searched For: modulus-of-elasticity-in-tension:[14000 TO 15000] brazing:"Good" CLEAR this search X SAVE this search << Page 1 2 >> 53 Alloys Found Alloy UNS#DesignationActiveView C33000 Low Leaded Brass (Tube) Yes C33000 Profile Suppliers of C33000 C33100 Leaded Brass No C33100 Profile Suppliers of C33100 C33200 High Leaded Brass (Tube) Yes C33200 Profile Suppliers of C33200 C33500 Low-Leaded Brass Yes C33500 Profile Suppliers of C33500 C34000 Medium Leaded Brass, 64-1/2% Yes C34000 Profile Suppliers of C34000 C34200 High Leaded Brass, 64-1/2% Yes C34200 Profile Suppliers of C34200 C34500 Yes C34500 Profile Suppliers of C34500 C35000 Medium Leaded Brass, 62% Yes C35000 Profile Suppliers of C35000 C35300 High Leaded Brass, 62% Yes C35300 Profile Suppliers of C35300 C35600 Extra High Leaded Brass Yes C35600 Profile Suppliers of C35600 C36000 Free-Cutting Brass Yes C36000 Profile Suppliers of C36000 C36010 Leaded Brass (Free-Cutting Brass) Yes C36010 Profile Suppliers of C36010 C36200 Leaded Brass No C36200 Profile Suppliers of C36200 C36500 Leaded Muntz Metal, Uninhibited Yes C36500 Profile Suppliers of C36500 C36600 Leaded Muntz Metal, Arsinical No C36600 Profile Suppliers of C36600 C36700 Leaded Muntz Metal, Antimonial No C36700 Profile Suppliers of C36700 C36800 Leaded Brass No C36800 Profile Suppliers of C36800 C37000 Free-Cutting Muntz Metal Yes C37000 Profile Suppliers of C37000 C37100 Yes C37100 Profile Suppliers of C37100 C37700 Forging Brass Yes C37700 Profile Suppliers of C37700 C38500 Architectural Bronze Yes C38500 Profile Suppliers of C38500 C45470 * Copper-Zinc-Tin Aluminum Alloy Yes C45470 Profile Suppliers of C45470 C48200 Naval Brass, Medium Leaded Yes C48200 Profile Suppliers of C48200 C48500 Naval Brass, High Leaded Yes C48500 Profile Suppliers of C48500 C49250 * Copper-Zinc-Bismuth (Copper-Zinc-Bismuth) Yes C49250 Profile Suppliers of C49250 C49300 * Lead-Free Bismuth Alloy (Lead-Free) Yes C49300 Profile Suppliers of C49300 C49340 * GEM Brass Yes C49340 Profile Suppliers of C49340 C49345 Low Leaded GEM Brass Yes C49345 Profile Suppliers of C49345 C49350 * Bismuth Brass Alloy Yes C49350 Profile Suppliers of C49350 C54400 Phosphor Bronze B-2 Yes C54400 Profile Suppliers of C54400 C67420 Yes C67420 Profile Suppliers of C67420 C69240 Yes C69240 Profile Suppliers of C69240 C83300 Yes C83300 Profile Suppliers of C83300 C84200 Yes C84200 Profile Suppliers of C84200 C84500 Yes C84500 Profile Suppliers of C84500 C84800 Plumbing Goods Brass Yes C84800 Profile Suppliers of C84800 C85800 Yes C85800 Profile Suppliers of C85800 C86550 Yes C86550 Profile Suppliers of C86550 C87900 Copper Silicon Yes C87900 Profile Suppliers of C87900 C90300 Tin Bronze Yes C90300 Profile Suppliers of C90300 C90500 Gun Metal Yes C90500 Profile Suppliers of C90500 C90700 Tin Bronze, 65 Yes C90700 Profile Suppliers of C90700 C91100 Yes C91100 Profile Suppliers of C91100 C91700 Nickel Gear Bronze Yes C91700 Profile Suppliers of C91700 C92300 Leaded Tin Bronze Yes C92300 Profile Suppliers of C92300 C92600 Yes C92600 Profile Suppliers of C92600 C92900 Yes C92900 Profile Suppliers of C92900 C93200 Yes C93200 Profile Suppliers of C93200 C93500 Yes C93500 Profile Suppliers of C93500 C93600 Yes C93600 Profile Suppliers of C93600 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 2 >>