Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
13 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C83400 |
Yes |
C83400 Profile Suppliers of C83400 |
|
C85300 |
Yellow Brass | No |
C85300 Profile Suppliers of C85300 |
C85500 |
Yes |
C85500 Profile Suppliers of C85500 |
|
C85700 |
Leaded Yellow Brass | Yes |
C85700 Profile Suppliers of C85700 |
C86100 |
Manganese Bronze | Yes |
C86100 Profile Suppliers of C86100 |
C86200 |
Yes |
C86200 Profile Suppliers of C86200 |
|
C86300 |
Manganese Bronze | Yes |
C86300 Profile Suppliers of C86300 |
C86400 |
Manganese Bronze | Yes |
C86400 Profile Suppliers of C86400 |
C86500 |
Manganese Bronze | Yes |
C86500 Profile Suppliers of C86500 |
C86700 |
Yes |
C86700 Profile Suppliers of C86700 |
|
C93600 |
Yes |
C93600 Profile Suppliers of C93600 |
|
C95200 * |
Yes |
C95200 Profile Suppliers of C95200 |
|
C95600 * |
Yes |
C95600 Profile Suppliers of C95600 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |