Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (19) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (6) You Searched For: modulus-of-elasticity-in-tension:[14000 TO 15000] electrical-conductivity:[15.0 TO 20.0] CLEAR this search X SAVE this search << Page 1 >> 19 Alloys Found Alloy UNS#DesignationActiveView C27460 Yes C27460 Profile Suppliers of C27460 C49300 * Lead-Free Bismuth Alloy (Lead-Free) Yes C49300 Profile Suppliers of C49300 C49340 * GEM Brass Yes C49340 Profile Suppliers of C49340 C49345 Low Leaded GEM Brass Yes C49345 Profile Suppliers of C49345 C49350 * Bismuth Brass Alloy Yes C49350 Profile Suppliers of C49350 C54400 Phosphor Bronze B-2 Yes C54400 Profile Suppliers of C54400 C67420 Yes C67420 Profile Suppliers of C67420 C84000 * Semi-Red Brass Yes C84000 Profile Suppliers of C84000 C84010 * Semi-Red Brass Yes C84010 Profile Suppliers of C84010 C84030 * Low Lead Semi-Red Brass Yes C84030 Profile Suppliers of C84030 C84200 Yes C84200 Profile Suppliers of C84200 C84500 Yes C84500 Profile Suppliers of C84500 C84800 Plumbing Goods Brass Yes C84800 Profile Suppliers of C84800 C85800 Yes C85800 Profile Suppliers of C85800 C86400 Manganese Bronze Yes C86400 Profile Suppliers of C86400 C86700 Yes C86700 Profile Suppliers of C86700 C87900 Copper Silicon Yes C87900 Profile Suppliers of C87900 C89535 Copper-Bismuth Alloy Yes C89535 Profile Suppliers of C89535 C93500 Yes C93500 Profile Suppliers of C93500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>