You Searched For:
12 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C27451 |
Yellow Brass (Yellow Brass) | Yes |
C27451 Profile Suppliers of C27451 |
C27460 |
Yes |
C27460 Profile Suppliers of C27460 |
|
C48600 |
DZR Brass | Yes |
C48600 Profile Suppliers of C48600 |
C49250 * |
Copper-Zinc-Bismuth (Copper-Zinc-Bismuth) | Yes |
C49250 Profile Suppliers of C49250 |
C67500 |
Manganese Bronze A | Yes |
C67500 Profile Suppliers of C67500 |
C67600 |
Yes |
C67600 Profile Suppliers of C67600 |
|
C84100 |
Yes |
C84100 Profile Suppliers of C84100 |
|
C85700 |
Leaded Yellow Brass | Yes |
C85700 Profile Suppliers of C85700 |
C85800 |
Yes |
C85800 Profile Suppliers of C85800 |
|
C86500 |
Manganese Bronze | Yes |
C86500 Profile Suppliers of C86500 |
C86550 |
Yes |
C86550 Profile Suppliers of C86550 |
|
C89838 |
Yes |
C89838 Profile Suppliers of C89838 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |