Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (31) Inactive Alloys (3) U.S. EPA Registered Antimicrobial (5) You Searched For: modulus-of-elasticity-in-tension:[14000 TO 15000] elongation:[24 TO 27] CLEAR this search X SAVE this search << Page 1 >> 34 Alloys Found Alloy UNS#DesignationActiveView C27450 Yellow Brass Yes C27450 Profile Suppliers of C27450 C27451 Yellow Brass (Yellow Brass) Yes C27451 Profile Suppliers of C27451 C27460 Yes C27460 Profile Suppliers of C27460 C28000 * Muntz Metal, 60% Yes C28000 Profile Suppliers of C28000 C33500 Low-Leaded Brass Yes C33500 Profile Suppliers of C33500 C34000 Medium Leaded Brass, 64-1/2% Yes C34000 Profile Suppliers of C34000 C34200 High Leaded Brass, 64-1/2% Yes C34200 Profile Suppliers of C34200 C34500 Yes C34500 Profile Suppliers of C34500 C35000 Medium Leaded Brass, 62% Yes C35000 Profile Suppliers of C35000 C35300 High Leaded Brass, 62% Yes C35300 Profile Suppliers of C35300 C35330 DZR Brass Yes C35330 Profile Suppliers of C35330 C35600 Extra High Leaded Brass Yes C35600 Profile Suppliers of C35600 C36000 Free-Cutting Brass Yes C36000 Profile Suppliers of C36000 C36010 Leaded Brass (Free-Cutting Brass) Yes C36010 Profile Suppliers of C36010 C36200 Leaded Brass No C36200 Profile Suppliers of C36200 C45470 * Copper-Zinc-Tin Aluminum Alloy Yes C45470 Profile Suppliers of C45470 C46400 Naval Brass, Uninhibited Yes C46400 Profile Suppliers of C46400 C46500 Naval Brass, Arsenical Yes C46500 Profile Suppliers of C46500 C46600 Tin Brass No C46600 Profile Suppliers of C46600 C46700 Tin Brass No C46700 Profile Suppliers of C46700 C48600 DZR Brass Yes C48600 Profile Suppliers of C48600 C49250 * Copper-Zinc-Bismuth (Copper-Zinc-Bismuth) Yes C49250 Profile Suppliers of C49250 C54400 Phosphor Bronze B-2 Yes C54400 Profile Suppliers of C54400 C67500 Manganese Bronze A Yes C67500 Profile Suppliers of C67500 C67600 Yes C67600 Profile Suppliers of C67600 C69240 Yes C69240 Profile Suppliers of C69240 C84030 * Low Lead Semi-Red Brass Yes C84030 Profile Suppliers of C84030 C84200 Yes C84200 Profile Suppliers of C84200 C86500 Manganese Bronze Yes C86500 Profile Suppliers of C86500 C87900 Copper Silicon Yes C87900 Profile Suppliers of C87900 C90500 Gun Metal Yes C90500 Profile Suppliers of C90500 C92200 Navy M Bronze Yes C92200 Profile Suppliers of C92200 C92300 Leaded Tin Bronze Yes C92300 Profile Suppliers of C92300 C94700 * Cast Nickel-Tin Bronze Yes C94700 Profile Suppliers of C94700 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>