Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (6) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (3) You Searched For: modulus-of-elasticity-in-tension:[14000 TO 15000] melting-point-liquidus:[1900 TO 2000] CLEAR this search X SAVE this search << Page 1 >> 6 Alloys Found Alloy UNS#DesignationActiveView C12600 Yes C12600 Profile Suppliers of C12600 C83300 Yes C83300 Profile Suppliers of C83300 C83400 Yes C83400 Profile Suppliers of C83400 C84000 * Semi-Red Brass Yes C84000 Profile Suppliers of C84000 C84030 * Low Lead Semi-Red Brass Yes C84030 Profile Suppliers of C84030 C95200 * Yes C95200 Profile Suppliers of C95200 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>