Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (3) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (0) You Searched For: modulus-of-elasticity-in-tension:[14000 TO 15000] melting-point-solidus:[1450 TO 1500] CLEAR this search X SAVE this search << Page 1 >> 3 Alloys Found Alloy UNS#DesignationActiveView C84100 Yes C84100 Profile Suppliers of C84100 C89535 Copper-Bismuth Alloy Yes C89535 Profile Suppliers of C89535 C89838 Yes C89838 Profile Suppliers of C89838 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>