Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (9) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (1) You Searched For: modulus-of-elasticity-in-tension:[16000 TO 17000] shrinkage-in-solidification:"Low" CLEAR this search X SAVE this search << Page 1 >> 9 Alloys Found Alloy UNS#DesignationActiveView C89325 Yes C89325 Profile Suppliers of C89325 C89835 * Federalloy III-932 Yes C89835 Profile Suppliers of C89835 C90200 Yes C90200 Profile Suppliers of C90200 C90900 Yes C90900 Profile Suppliers of C90900 C91000 Yes C91000 Profile Suppliers of C91000 C91300 Yes C91300 Profile Suppliers of C91300 C92500 Yes C92500 Profile Suppliers of C92500 C92700 Leaded Tin Bronze Yes C92700 Profile Suppliers of C92700 C92800 Yes C92800 Profile Suppliers of C92800 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>