Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (3) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (3) You Searched For: modulus-of-elasticity-in-tension:[17000 TO 18000] capacity-for-being-cold-worked:"Fair" CLEAR this search X SAVE this search << Page 1 >> 3 Alloys Found Alloy UNS#DesignationActiveView C14750 * High Copper Alloy Yes C14750 Profile Suppliers of C14750 C61800 * Yes C61800 Profile Suppliers of C61800 C63200 * Aluminum Bronze Yes C63200 Profile Suppliers of C63200 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>