Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (7) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (6) You Searched For: modulus-of-elasticity-in-tension:[17000 TO 18000] soldering:"Not Recommended" CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C60800 Yes C60800 Profile Suppliers of C60800 C61300 * Yes C61300 Profile Suppliers of C61300 C61400 * Yes C61400 Profile Suppliers of C61400 C62300 * Aluminum Bronze, 9% Yes C62300 Profile Suppliers of C62300 C62400 * Aluminum Bronze,11% Yes C62400 Profile Suppliers of C62400 C63000 * Aluminum Bronze Yes C63000 Profile Suppliers of C63000 C99300 * Incramet 800 Yes C99300 Profile Suppliers of C99300 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>