Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (2) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (2) You Searched For: modulus-of-elasticity-in-tension:[19000 TO 20000] melting-point-liquidus:[1600 TO 1700] CLEAR this search X SAVE this search << Page 1 >> 2 Alloys Found Alloy UNS#DesignationActiveView C49355 * Copper Zinc Bismuth Alloy Yes C49355 Profile Suppliers of C49355 C87800 * Cast Silicon Bronze Yes C87800 Profile Suppliers of C87800 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>