Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (8) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (9) You Searched For: rockwell-30t-scale:[55 TO 60] tensile-strength:[100 TO 110] CLEAR this search X SAVE this search << Page 1 >> 9 Alloys Found Alloy UNS#DesignationActiveView C17000 * Copper Beryllium Yes C17000 Profile Suppliers of C17000 C17200 * Copper Beryllium Yes C17200 Profile Suppliers of C17200 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C41100 * Tin Brass Yes C41100 Profile Suppliers of C41100 C64400 * Aluminum Bronze No C64400 Profile Suppliers of C64400 C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 C66900 * Manganese Brass Yes C66900 Profile Suppliers of C66900 C72500 * Yes C72500 Profile Suppliers of C72500 C74500 * Nickel Silver, 65-10 Yes C74500 Profile Suppliers of C74500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>