Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (6) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (7) You Searched For: rockwell-b-scale:[40 TO 50] modulus-of-elasticity-in-tension:[18000 TO 19000] CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C17500 * Copper Beryllium Yes C17500 Profile Suppliers of C17500 C19000 * Yes C19000 Profile Suppliers of C19000 C40500 * Penny Bronze Yes C40500 Profile Suppliers of C40500 C40800 * Silicon Brass No C40800 Profile Suppliers of C40800 C41100 * Tin Brass Yes C41100 Profile Suppliers of C41100 C75200 * Nickel Silver, 65-18 Yes C75200 Profile Suppliers of C75200 C75700 * Nickel Silver, 65-12 Yes C75700 Profile Suppliers of C75700 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>