Saved Copper Alloys

Saved Searches

Copper Alloy Advanced Search Help

We'd Love Your Input

Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.

3 Alloys Found

Alloy UNS#DesignationActiveView

C48200

Naval Brass, Medium Leaded Yes C48200 Profile
Suppliers of C48200

C70600 *

Copper-Nickel, 10% Yes C70600 Profile
Suppliers of C70600

C85570

Yes C85570 Profile
Suppliers of C85570
* signifies an alloy registered with the U.S. EPA as Antimicrobial.