14 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C15720 * |
Dispersion Strengthned Alloy | Yes |
C15720 Profile Suppliers of C15720 |
C15750 * |
Dispersion Strengthened Copper (C3/60) | Yes |
C15750 Profile Suppliers of C15750 |
C15760 * |
Dispersion Strengthened Alloy | Yes |
C15760 Profile Suppliers of C15760 |
C17000 * |
Copper Beryllium | Yes |
C17000 Profile Suppliers of C17000 |
C17200 * |
Copper Beryllium | Yes |
C17200 Profile Suppliers of C17200 |
C17500 * |
Copper Beryllium | Yes |
C17500 Profile Suppliers of C17500 |
C17510 * |
Copper Beryllium | Yes |
C17510 Profile Suppliers of C17510 |
C67400 |
Yes |
C67400 Profile Suppliers of C67400 |
|
C67500 |
Manganese Bronze A | Yes |
C67500 Profile Suppliers of C67500 |
C82000 * |
Copper Beryllium 10C | Yes |
C82000 Profile Suppliers of C82000 |
C86700 |
Yes |
C86700 Profile Suppliers of C86700 |
|
C89720 * |
Copper-Bismuth Alloy (TECO) | Yes |
C89720 Profile Suppliers of C89720 |
C95200 * |
Yes |
C95200 Profile Suppliers of C95200 |
|
C99750 |
Yes |
C99750 Profile Suppliers of C99750 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |