Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (8) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (8) You Searched For: rockwell-b-scale:[70 TO 80] elongation:[18 TO 21] gas-shielded-arc-welding:"Excellent" CLEAR this search X SAVE this search << Page 1 >> 8 Alloys Found Alloy UNS#DesignationActiveView C19200 * Yes C19200 Profile Suppliers of C19200 C65100 * Low-Silicon Bronze B Yes C65100 Profile Suppliers of C65100 C65500 * High-Silicon Bronze A Yes C65500 Profile Suppliers of C65500 C70400 * Copper-Nickel, 5% Yes C70400 Profile Suppliers of C70400 C71000 * Copper-Nickel, 20% Yes C71000 Profile Suppliers of C71000 C87600 * Copper Silcon Alloy Yes C87600 Profile Suppliers of C87600 C87610 * Cast Copper-Silicon Yes C87610 Profile Suppliers of C87610 C95200 * Yes C95200 Profile Suppliers of C95200 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>