Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (6) You Searched For: rockwell-b-scale:[70 TO 80] elongation:[51 TO 54] tensile-strength:[100 TO 110] coated-metal-arc-welding:"Not Recommended" CLEAR this search X SAVE this search << Page 1 >> 6 Alloys Found Alloy UNS#DesignationActiveView C16200 * Cadmium Copper Yes C16200 Profile Suppliers of C16200 C16210 * High Copper Alloy No C16210 Profile Suppliers of C16210 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>